1 / 3 · 点击缩略图查看
IVOCLAR-096
Ivoclar Minigold
Minigold
📝 综合简介
Ivoclar Minigold是一种Au含量40.0%、Pd 4.0%、Ag 47.0%的Type 4贵金属铸造合金,符合ISO 22674:2016标准,呈金黄色。该合金密度为12.4 g/cm³,熔化范围865 - 945 °C,弹性模量88 GPa。其铸态维氏硬度19
① 专业规格
- 品牌
- Ivoclar
- 官网
- https://www.ivoclar.com/en_us/products/alloys/minigold
- 来源
- 厂家官网公开信息(Playwright 采集 2026-08)· 客观整理 · 未实测
- 分类段
- alloys
- 落地步骤
- ② 设计(CAD)
- 厂家参数原文
- Minigold® Au (40.0%)-based dental casting alloy, Type 4 Purchase Online Today Minigold is a gold-reduced casting alloy. Its composition makes it suitable for a wide range of indications and its golden yellow colour allows natural shade effects in the restoration veneered with laboratory composite SR Nexco. Indications* Onlays, ¾ crowns, crowns Telescope crowns, conus crowns Bridges Wide-span bridges Cast posts / cores, bars, attachments Technical Data Composition (%): Au 40.0 | Pd 4.0 | Ag 47.0 | Cu 7.5 | Zn 1.0 | In <1.0, Ir <1.0 ISO 22674:2016 ADA Type Noble Type / Color 4 / Yellow Density (g/cm³) 12.4 Melting Range (Solidus/Liquidus): 865 - 945 °C Elastic Modulus (GPa): 88 As Cast Softened Hardened Vickers Hardness: 190 125 215 Tensile Strength (MPa): 600 400 680 0.2% Proof Stress (MPa): 430 280 540 Elongation (%): 15 30 12 Advantages Golden yellow colour Wide range of indications Veneering with laboratory composites (e.g. SR Nexco) Excellent resistance to oral conditions Tested biocompatibility Processing Data Investment Material: Phosphate-bonded / Gypsum-bonded Preheating / Burn- out Temperature: 650 - 760 °C Crucible Carbon crucible / Ceramic crucible Casting Temperature: 1000 - 1050 °C Recommended Lab Composite: SR Nexco Laser Welding Wire: Laser C&B Yellow *See TYPE CLASSIFICATION DUE TO PHYSICAL PROPERTIES Download Materials Get this product in our online shop Buy now in our Online Shop with your Ivoclar webshop account Click here to go to the online shop TOP --- Composition (%): Au 40.0 | Pd 4.0 | Ag 47.0 | Cu 7.5 | Zn 1.0 | In <1.0, Ir <1.0 ISO 22674:2016 ADA Type Noble Type / Color 4 / Yellow Density (g/cm³) 12.4 Melting Range (Solidus/Liquidus): 865 - 945 °C Elastic Modulus (GPa): 88 As Cast Softened Hardened Vickers Hardness: 190 125 215 Tensile Strength (MPa): 600 400 680 0.2% Proof Stress (MPa): 430 280 540 Elongation (%): 15 30 12 --- Investment Material: Phosphate-bonded / Gypsum-bonded Preheating / Burn- out Temperature: 650 - 760 °C Crucible Carbon crucible / Ceramic crucible Casting Temperature: 1000 - 1050 °C Recommended Lab Composite: SR Nexco Laser Welding Wire: Laser C&B Yellow
⑤ 贸易信息(HS / 原产地 / 认证)
- HS 编码
- —
- 原产地
- CN
- 资质认证
- —
⑥ 定制 / 起订 / 交期
- MOQ
- 1000
- 交期
- —
—
⑦ 合规标注
—
⑧ 知识底座 · 选这件你该懂的专业知识
【Ivoclar 全目录采集】https://www.ivoclar.com/en_us/products/alloys/minigold
由平台品类知识库提供专业解读,帮你看懂面料/工艺/法规 · 随品类持续沉淀扩充。
AustinEco · 工厂级专业规格 · 全球 192 国直供 · 本页价格信息不对外展示,询价请走平台业务通道。